Wood pulp

Bleached sulfate cellulose from a mixture of hardwood species LSO, LS1 according to GOST 28172-89

Article ID
CT-188
Category
Wood pulp
Standard
GOST 28172-89

Price on request. The cost is calculated individually, taking into account volumes, packaging and delivery region.

Request a quote →

Description and specifications

Resistance

Characteristics LS 0
(HIGHEST GRADE)
LS 0
(FIRST GRADE)
LS 1
(HIGHEST GRADE)
LS 1
(FIRST GRADE)
Mechanical strength when milled in a CRA mill to 60° SR.        
— Breaking length, km, not less than 7.5 6.8 8 7.1
— Absolute tearing resistance, cN, not less than 47 47 44 44
— Folding endurance (number of double folds), not less than 300 300 300 300
Whiteness, %, not less than 89 89 87 87
Dirt count, number of specks with an area of:        
— from 0.1 to 1.00 mm², inclusive, not more than 30 34 45 50
— from 1.0 to 2.00 mm², inclusive, not more than 1 2 2 3
— over 2.0 mm² 0 0 0 0
pH of aqueous extract 5.0-7.0 5.0-7.0 5.0-7.0 5.0-7.0
Moisture, %, not more than 20 20 20 20

Manufacture of LS-2, LS-3, LS-4 according to GOST 28172-89 is available on request.

Shipping:

  • Shipping by rail, road, or sea is possible.
  • Road transport: max. 20 tons
  • Rail transport: max. 63 tons

Packaging:

  • Bale wrapped in two layers of bleached cardboard and bound with wire.
  • Weight: 200 kg
  • Dimensions: 60x80x45 cm

Enquire about: Bleached sulfate cellulose from a mixture of hardwood species LSO, LS1 according to GOST 28172-89

Fill in the form — your e-mail client will open with a pre-filled message to cardenostrade@gmail.com. We reply with pricing, specifications and delivery terms.